Metallographic GIGA-S Vibratory Polishers Specifications

Feature GIGA-S
Polishing Bowl size 9 and/or 12-inch diameter
Drive Mechanism Horizontal frequency control,
PZT variable voltage control
Construction Aluminum casting,
FRP (reinforced plastic)
cover and acrylic hood
Electrical Specifications 110V or 220V 50/60 Hz
Frequency 1-220 Hz
Dimensions
(W x D x H)
430 mm x 525 mm x 410 mm
17 x 21 x 16-inches
Weight 135 lbs (62 kgs)
Part No. GIGA-S
Brochures Metallographic Vibratory Polishing Machines

Return to top


Copyright 2006-2022
PACE TECHNOLOGIES® - 3601 E. 34th St., Tucson, AZ 85713, USA
Telephone +1-520-882-6598 FAX +1-520-882-6599
All Rights Reserved


PACE Technologies facebook link Blog us on Tumblr Blog us on Tumblr PACE Technologies LinkIn PACE Technologies YouTube Videos