Description:
Tough engineering ceramics such as silicon nitride and zirconia continue to find industrial applications where strength or wear resistance is required, oftentimes at relatively high operating temperatures.

Preparation Challenge:
Engineering ceramics are very hard, therefore specimen preparation procedures generally use a CMP (chemical mechanical polishing) component to remove induced microstructural damage.

Metallographic microstructure of partially stabilized zirconia
Metallographic microstrucuture of Silcon nitride
Metallographic microstructure of SiSiC engineered ceramic
Metallographic microstructure SIALON