NANO-1000S / FEMTO-1500S Auto Polisher![]() |
Feature | FEMTO 1100S Individual Force Auto Polishers |
FEMTO 1500S Individual Force Auto Polishers |
---|---|---|
Application of Force | Independent pistons | Individual pistons) Central force |
Head speed | 0-300 rpm (variable) | 0-300 rpm (variable) |
Samples | 1-6 | 1-6 |
Force | 1.1 - 13.5 lbs (5- 60 N) (5- 60 N) |
1.1 - 13.5 lbs (5- 60 N) (5- 60 N) |
Compatibility | NANO 1000S polishers (8 & 10-inch Polishers) |
NANO 1000S polishers (8 & 10-inch Polishers) |
Construction | SMC injection plastic | SMC injection plastic |
Electrical Specifications | 110V/220V, 50/60 Hz | 110V/220V, 50/60 Hz |
Dimensions (W x D x H) |
9.4 x 12.6 x 20 inch (240 x 320 x 520 mm) |
9.4 x 12.6 x 20 inch (240 x 320 x 520 mm) |
Weight | 60 lbs (28 kg) without polisher base |
60 lbs (28 kg) without polisher base |
Specimen Holder | Individual | Individual / Central |
Brochure | ![]() |
![]() |