Wheel feed cutters MEGA-T400 Abrasive Saw
MEGA-T400 16-inch Abrasive Saw
Click here to get a quote

Metallographic MEGA-T400 Specifications

Feature MEGA-T400 Description MEGA-T400V Description
Cut-off blade size Max diameter 16-inch (400 mm) Max diameter 16-inch (400 mm)
Cutting capacity Max diameter 6-inch (150 mm) Max diameter 6-inch (150 mm)
Wheel feed Manual Manual
Table feed Yes Yes
T-slotted
Table Dimensions
14.6 x 14.2-inch
(370 mm x 360 mm)
14.6 x 14.2-inch
(370 mm x 360 mm)
Operation Manual Manual
Cooling Unit 16 gallons (60 liters) 16 gallons (60 liters)
Motor power 7.5 hp (5.3 KW), 2800 rpm 7.5 hp (5.3 KW), 2800 rpm
Motor speed 2910 rpm at 208-380V/50 Hz
3492 rpm at 208-380V/60 Hz
1455 rpm at 440-480V/50 Hz
1740 rpm at 440-480V/60 Hz

Optional variable speed (MEGA-T400V)
2910 rpm at 208-380V/50 Hz
3492 rpm at 208-380V/60 Hz
1455 rpm at 440-480V/50 Hz
1740 rpm at 440-480V/60 Hz
Electrical Specification Standard 480 3-phase
(208Y, 380V or 440V 3-phase optional), 50/60 Hz
Standard 480 3-phase, 50/60 Hz
Dimensions (WxDxH) 50 x 39 x 64-inch
(127 cm x 99 cm x 160 cm) (hood closed)

50 x 39 x 83-inch
(127 cm x 99 cm x 211 cm (hood open)
50 x 39 x 64-inch
(127 cm x 99 cm x 160 cm) (hood closed)

50 x 39 x 83-inch
(127 cm x 99 cm x 211 cm (hood open)
Weight 700 lbs (300 kg) 700 lbs (300 kg)
Part No. MEGA-T400 MEGA-T400V

Return to top

Copyright 2006-2021
PACE Technologies ® - 3601 E. 34th St., Tucson, AZ 85713, USA
Telephone +1-520-882-6598 FAX +1-520-882-6599
All Rights Reserved


PACE Technologies facebook link Blog us on Tumblr Blog us on Tumblr PACE Technologies LinkIn PACE Technologies YouTube Videos