Description:

Glasses and minerals are generally fairly hard and have a tendency to fracture.

Preparation Challenge:

Proper specimen preparation requires that the damage during specimen preparation be minimized, even as early as the sectioning or cutting operation.

Examples:
GLASS & MINERAL PROCEDURES
Alumino-silicate glass
Metallographic microstructure of alumino-silicate glass

Graphite
Metallographic microstructure of graphite

Slag
Metallographic microstructure of slag

Periclase mineral
Metallographic micrograph of Periclase

Chalcopyrite mineral
Metallographic micrograph of chalcopyrite

 

PACE TECHNOLOGIES CONTACT


PACE Technologies
3601 E. 34th St.
Tucson, Arizona 85713
+1-520-882-6598
FAX +1-520-882-6599
email: pace@metallographic.com
www.metallographic.com


Information Requests

*Required Information

*Company:
*Name:
*E-mail:
Title:
*Address:
P.O. / Suite:
*City:
*State:
*Zip Code:
Country:
*Phone:
Fax:

Industry:

Process Type:

Send Equipment Quotes
Add my name to PACE Technologies mailing list
Send NEW 2018-2020 Product catalog
Send me my FREE MET MANUAL (with $50 order)
Request a salesperson call

Metallographic
Consumables

Brochures:

For online
ordering
click here
Online Ordering
Abrasive Blades
Diamond Blades
Compression Mounting
Castable Mounting
Polishing Pads
Lapping Films
Diamond Disks
Composite Disks
Polycrystalline Diamond
Monocrystalline Diamond
Final Polishing Abrasives
Etchants
Consumables Catalog

Metallographic
Equipment

Brochures:

For specific
equipment quotes
click here
Quotes
Abrasive Cutters
Precision Wafering Saws
Compression Mounting Presses
Castable Vacuum Chamber
Manual Roll and Belt Grinders
Polishing Machines
Automated Polishing Heads
Vibratory Polisher

Metallographic
Analysis
Brochures:

For specific
instrument quotes
click here
Quotes
Microscopes
Microhardness Testers
Rockwell Hardness Testers
Brinell Hardness Testers
MacroVickers Hardness Tester
Image Analysis

Laboratory
Furniture
Brochures:

For specific
items quotes
click here
Quotes
Lab Benches
Microscope Benches
Fume Hood
Safety Cabinets
Specimen Storage Cabinet

Other Questions

Question To:
Enter Request Info. or Question:



Copyright 2006-2019
PACE Technologies ® - 3601 E. 34th St., Tucson, AZ 85713, USA
Telephone +1-520-882-6598 FAX +1-520-882-6599
All Rights Reserved


PACE Technologies facebook link Blog us on Tumblr Blog us on Tumblr PACE Technologies Google+ PACE Technologies Google+