PACE Technologies logo PACE Technologies web collage PACE Technologies best price guarantee logo



Click here to get a quote

Metallographic Precision Wafering Saws

Metallographic medium speed precision wafering saw Metallographic medium speed precision wafering saw Metallographic table feed precision wafering saw
Wafering Saws PICO 155 / PICO 155P PICO 175 PICO 200
Blade size 3-6 inch (75-150 mm) 3-7 inch (75 -175 mm) 8-inch (200 mm)
Cutting Capacity (max.) 2-inch (50 mm) 2.4-inch (60 mm), 4-inch (100 mm) with specimen rotation 1.5-inches (38 mm)
Coolant Gravity / Pump Auto Gravity
Variable Speed (rpm) 50-1500 rpm 50-5000 rpm 300-3000 rpm
Fixtures PICO 155 fixtures PICO 175 fixtures PICO 200 fixtures
Part No. PICO 155P PICO 175 PICO 200

PICO 155 Low to Medium Speed Precision Cutter gravity feed coolant

Medium speed precision wafering saw

 

Metallographic medium speed precision wafering saw Click here to get a quote
Feature PICO 155 Description
Cutting capacity Max diameter 2-inch (50 mm)
Coolant Gravity drag
Cut-off blade size 3-inch (75 mm) - 7-inch (175 mm)
Arbor size 0.5-inch (12.7 mm)
Variable Speed (rpm) 50-1500 rpm continuously adjustable with LED speed display
Cutting Load 0-1500 gram load
Micrometer feed distance 0 to 1-inch (0-25 mm)
Micrometer accuracy 2 microns
Motor power 125W (24V)
Electrical Specification 110V/220V (50/60 Hz) (single phase)
Dimensions
(W x D x H)

Hood closed: 19.5 x 22.5 x 15-inch
(495 x 570 x 375 mm)

Hood open 19.5 x 22.5 x 21-inch
(495 x 570 x 540 mm)

Weight 66 lbs (30 kg)
PICO 155 fixtures PICO 155 fixtures

PICO 155P Low to Medium Speed Precision Cutter with coolant pump (Part Number PICO-155P)

Medium speed precision wafering saw

 

Metallographic medium speed precision wafering saw Click here to get a quote
Feature PICO 155P Description
Cutting capacity Max diameter 2-inch (50 mm)
Coolant Dual nozzle with pump
Cut-off blade size 3-inch (75 mm) - 7-inch (175 mm)
Arbor size 0.5-inch (12.7 mm)
Variable Speed (rpm) 50-1500 rpm continuously adjustable with LED speed display
Cutting Load 0-1500 gram load
Micrometer feed distance 0 to 1-inch (0-25 mm)
Micrometer accuracy 2 microns
Motor power 125W (24V)
Electrical Specification 110V/220V (50/60 Hz) (single phase)
Dimensions
(W x D x H)
Hood closed:19 x 23 x 14.5-inch
(480 x 580 x 368 mm Hood open: 19 x 29 x 19-inch
(480 x 740 x 370 mm)
Weight 66 lbs (30 kg)
PICO 155P fixtures PICO 155P fixtures

PICO 175 High Speed Precision Cutter with coolant pump (Part Number PICO-175)

High speed precision wafering saw

 

Metallographic medium speed precision wafering saw Click here to get a quote
Feature PICO 175 Cutter Description
Cutting capacity 3-inches (75 mm)
Cut-off blade size Min 3-inch (75 mm)
Max 8-inch (200 mm)
Arbor size 0.5-inch (12.7 mm)
Travel Distances X-direction: 0-2.6 inches( 0-66 mm)
Y-direction: 0-3.4 (0-86mm)
Variable Speed (rpm) 50-5000 rpm continuously adjustable
Feed Rate 0.0024-7.1 inches/minute (0.01-3 mm/second)
Cutting Load 5-20 N (1-4.5 lbf)
Micrometer feed distance 0 to 4-inch (0-100 mm)
Micrometer accuracy 0.1 mm
Motor power 1.0 hp (750 W)
Electrical Specification 110V or 220V (50/60 Hz) (single phase)
Dimensions
(W x D x H)
Hood closed: 25 x 22.4 x 17.8-inch
(635 x 570 x 450-mm) Hood open: 25 x 23 x 29-inch
(635 x 585 x 740 mm
Weight 160 lbs (35 kg)
PICO 175 fixtures PICO 175 fixtures

PICO 155/175 Fixtures and Accessories

Description Part Number PICO 155/155P PICO 175 Image
Universal specimen vise P150-702 x x PICO 155 universal holder
Large single saddle vise with lip P150-702b x x PICO 155 Large single saddle vise with lip
Sample holder with double parallel vise for long specimens P150-703 x x PICO 155 Sample holder wit double parallel vise for long specimens
Sample holder for round and mounted specimens (1.25-inch) P150-707 x x PICO 155 Sample holder for round and mounted specimens
Teardrop holder (18-40 mm)(0.7-1.6-inch) P150-710 x x PICO 155 Teardrop holder
Specimen vise for irregular shaped specimens P150-706 x x PICO 155 Specimen vise for irregular shaped specimens
Specimen vise for adhering specimens P150-709 x x PICO 155 Specimen vise for adhering specimens
Swivel arm unit for angular cutting P150-705 x PICO 155 Swivel arm unit for angular cutting
Fastener vise for longitudinal sectioning for fasteners, tubes etc. P150-711 x x PICO 155 Fastener vise for longitudinal sectioning for fasteners, tubes etc
50 mm diameter flanges P150-306 x x PICO 155 50 mm diameter flanges
75 mm diameter flanges P150-712 x x PICO 155 75 mm diameter flanges
Cutting table attachment for manual cutting of printed circuit board specimens P150-601 x n.a PICO 155 Cutting table attachment for manual cutting of printed circuit board specimens
Wafering blade dressing fixture, PICO 155 saws P150-701 x n.a PICO 155 Wafering blade dressing fixture
Wafering blade dressing fixture, PICO 175 saw P175-DF n.a x PICO 155 Wafering blade dressing fixture
Dovetail adapter for PICO 175 P175-750 n.a. x PICO 175 dove tail adapter
Locking blade rod for PICO 175 P175-755 n.a x PICO 175 locking handle


The PICO 200 Variable Speed Table Saw (Part No. PICO-200)

Table feed precision wafering saw

 

Metallographic medium speed precision wafering saw Click here to get a quote
Feature PICO 200 Description
PICO 200 Description Specification
Cutting capacity 1.5-inches (38 mm)
Specimen feed Table feed
Coolant tank 3 Liters
Cut-off blade size 8-inch (200 mm)
Arbor size 0.5-inch
Variable Speed (rpm) 300-3000 rpm continuously adjustable with LED speed display
Motor power 1.0 hp (750 W)
Electrical Specification 110V/220V (50/60 Hz) (single phase)
Dimensions
(W x D x H)
18 x 20 x 13.8-inch
(460 x 500 x 350 mm)
Weight 93 lbs (42 kg)
PICO 200 fixtures PICO 200 fixtures

PICO 200 Fixtures and Accessories

PICO 200 Fixtures Part No.
PICO 200 Fixtures Part No.
Vertical clamping vise with shoe P200-V
Height adapter for P200-V vertical clamping vises P200-H
Angle cutting guide P200-ANGLE
Vacuum cleaning attachment P200-VAC

PACE TECHNOLOGIES CONTACT


PACE Technologies
3601 E. 34th St.
Tucson, Arizona 85713
+1-520-882-6598
FAX +1-520-882-6599
email: pace@metallographic.com
www.metallographic.com


Information Requests

*Required Information

*Company:
*Name:
*E-mail:
Title:
*Address:
P.O. / Suite:
*City:
*State:
*Zip Code:
Country:
*Phone:
Fax:

Industry:

Process Type:

Send Equipment Quotes
Add my name to PACE Technologies mailing list
Send NEW 2018-2020 Product catalog
Send me my FREE MET MANUAL (with $50 order)
Request a salesperson call

Metallographic
Consumables

Brochures:

For online
ordering
click here
Online Ordering
Abrasive Blades
Diamond Blades
Compression Mounting
Castable Mounting
Polishing Pads
Lapping Films
Diamond Disks
Composite Disks
Polycrystalline Diamond
Monocrystalline Diamond
Final Polishing Abrasives
Etchants
Consumables Catalog

Metallographic
Equipment

Brochures:

For specific
equipment quotes
click here
Quotes
Abrasive Cutters
Precision Wafering Saws
Compression Mounting Presses
Castable Vacuum Chamber
Manual Roll and Belt Grinders
Polishing Machines
Automated Polishing Heads
Vibratory Polisher

Metallographic
Analysis
Brochures:

For specific
instrument quotes
click here
Quotes
Microscopes
Microhardness Testers
Rockwell Hardness Testers
Brinell Hardness Testers
MacroVickers Hardness Tester
Image Analysis

Laboratory
Furniture
Brochures:

For specific
items quotes
click here
Quotes
Lab Benches
Microscope Benches
Fume Hood
Safety Cabinets
Specimen Storage Cabinet

Other Questions

Question To:
Enter Request Info. or Question:



Copyright 2006-2019
PACE Technologies ® - 3601 E. 34th St., Tucson, AZ 85713, USA
Telephone +1-520-882-6598 FAX +1-520-882-6599
All Rights Reserved


PACE Technologies facebook link Blog us on Tumblr Blog us on Tumblr PACE Technologies Google+ PACE Technologies Google+