The applications for lapping films range from polishing semiconductor dies, fiber optics, optical components, ceramic capacitors, computer hard drive read-write heads, ceramic seals, etc. The main characteristic of lapping films is that they produce very flat surfaces, especially across materials with a wide range in hardness.
PACE Technologies Lapping Films
Lapping films are precision-coated abrasives used for producing extremely flat surfaces across diverse materials such as semiconductor dies, fiber optics, ceramic capacitors, optical components, and hard drive read-write heads. Their uniform abrasive distribution makes them ideal for applications requiring consistent surface finishes, even across varying material hardnesses.
These films are composed of a durable polyester backing (typically 3 mils) with abrasives fixed in place using an epoxy or adhesive binder. Common abrasive types include diamond, silicon carbide, alumina, and occasionally ceria, selected based on application requirements.
Diamond lapping films use precisely graded diamond abrasives bonded with a flexible, solvent-resistant adhesive. They offer a fixed-abrasive polishing mode, reduced relief compared to cloths, and are excellent for preparing microelectronic specimens for SEM and TEM analysis.
Silicon carbide lapping films feature sharp, angular particles aligned to provide high stock removal rates and minimal damage. These films continuously expose fresh abrasives, making them highly efficient for rapid material removal.
Alumina lapping films utilize aluminum oxide in either the softer gamma or harder alpha phase (up to 2000 HV). These films are typically used for final polishing due to their hardness, consistency, and surface finish quality.
| Symptom | Cause | Action |
|---|---|---|
| Coarse scratching | -Swarf build-up on the lapping film | -Use a lubricant with an appropriate surfactant |
| Tearing of pad | -Sharp specimen edges | -Reduce intitial applied load so that the specimen edge does not cut the film. Gradually increase pressure during the lapping operation. -Dispense lubricant more frequently |
| Excessive relief or edge rounding | -PSA backing providing too much flexibility (resiliency) -Lapping backing plate surface is not flat |
-Use a plain backed diamond lapping film -Use a flat lapping surface |
| Description | Size (inches) | Catalog Number (Plain-backed) | Catalog Number (PSA backed) | Color Code |
|---|---|---|---|---|
| 0.10 um Diamond Lapping Film | Up to 12-inches | DA-01 | DAA-01 | ![]() |
| 0.25 um Diamond Lapping Film | Up to 12-inches | DA-025 | DAA-025 | ![]() |
| 0.50 um Diamond Lapping Film | Up to 12-inches | DA-052 | DAA-05 | ![]() |
| 1 um Diamond Lapping Film | Up to 12-inches | DA-1 | DAA-1 | ![]() |
| 3 um Diamond Lapping Film | Up to 12-inches | DA-3 | DAA-3 | ![]() |
| 6 um Diamond Lapping Film | Up to 12-inches | DA-6 | DAA-6 | ![]() |
| 9 um Diamond Lapping Film | Up to 12-inches | DA-9 | DAA-9 | ![]() |
| 15 um Diamond Lapping Film | Up to 12-inches | DA-15 | DAA-15 | ![]() |
| 30 um Diamond Lapping Film | Up to 12-inches | DA-30 | DAA-30 | ![]() |
| Description | Quantity (oz) | Catalog Number |
|---|---|---|
| 32 oz Diamond Lapping Film Lube | 32 | LFL-032 |
| 1 gallon Diamond Lapping Film Lube | 128 | LFL-128 |
| Description | Size (inches) | Catalog Number (Plain-backed) | Catalog Number (PSA backed) |
|---|---|---|---|
| 1.0 um silicon carbide | Up to 12-inches | SIC-001PB-3 | SIC-001PSA-3 |
| 3.0 um silicon carbide | Up to 12-inches | SIC-003PB-3 | SIC-003PSA-3 |
| 5.0 um silicon carbide | Up to 12-inches | SIC-005PB-3 | SIC-005PSA-3 |
| 9.0 um silicon carbide | Up to 12-inches | SIC-009PB-3 | SIC-009PSA-3 |
| 12 um silicon carbide | Up to 12-inches | SIC-012PB-3 | SIC-012PSA-3 |
| 20 um silicon carbide | Up to 12-inches | SIC-020PB-3 | SIC-020PSA-3 |
| 30 um silicon carbide | Up to 12-inches | SIC-030PB-3 | SIC-030PSA-3 |
| Description | Size (inches) | Catalog Number (Plain-backed) | Catalog Number (PSA backed) | Color Code |
|---|---|---|---|---|
| 0.05 um alumina (ALO) | Up to 12-inches | ALO-105PB-3 | ALO-105PSA-3 | ![]() |
| 0.30 um alumina | Up to 12-inches | AL-103PB-3 | AL-103PSA-3 | ![]() |
| 1.0 um alumina | Up to 12-inches | AL-001PB-3 | AL-001PSA-3 | ![]() |
| 3.0 um alumina | Up to 12-inches | AL-003PB-3 | AL-003PSA-3 | ![]() |
| 5.0 um alumina | Up to 12-inches | AL-005PB-3 | AL-005PSA-3 | ![]() |
| 9.0 um alumina | Up to 12-inches | AL-009PB-3 | AL-009PSA-3 | ![]() |
| 12 um alumina | Up to 12-inches | AL-012PB-3 | AL-012PSA-3 | ![]() |
| 15 um alumina | Up to 12-inches | AL-015PB-3 | AL-015SA-3 | ![]() |
| 30 um alumina | Up to 12-inches | AL-030PB-3 | AL-030PSA-3 | ![]() |